effetre silver black and powder pink

Started by flowerjasper, March 03, 2010, 12:02:53 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

flowerjasper

has anyone tried these two yet? not necessarily together !
am not having much luck with either  :(
sandy

hollergrafik

silver black is shocky, spitty, nasty glass that doesnt do much, powder pink goes a really weird colour for me, kinda sickly skin colour.

tuffnell glass

Hi ,
      We both worked with Silver black on Sunday at Essex Beadfair on a Minor and a Hot head , the black worked really nice ,easily reducing as you work with ith it . The sticks we worked with were not shocky at all .

I'll try to have a go with the powder pink today to see what happens .

Cheers ,

martin

tuffnellglass@yahoo.co.uk
www.tuffnellglass.com
www.flameoff.co.uk

Lush!

I used Silver Black a couple of days ago - it wasn't particularly shocky, reduced really easily, great gunmetal effect.  Does pit though, you have to keep moving up the flame with it.

Its the bead in the middle here



www.lushlampwork.etsy.com

Mand

I've just bought some silver black from Tuffnells and I love it. I think Kaz had some mega shocky stuff a while back which sh edidn't get on with?

hollergrafik

I am gonna give it another go then, warm them on the kiln see what they do

Dragonfire Glass

Powder pink is one of my favourite glass colours - love the different shades you can get from it.
Haven't tried silver black.

Sulis (Hazel)

I just bought some silver black on recommendation from a lovely lady I know. If I can get to the torch tonight I'll let you know how it goes. Mine was from Martin.

:-*
Hazel x

flowerjasper

that middle bead looks great julie, i must give them another go,
sandy x

tuffnell glass


tuffnellglass@yahoo.co.uk
www.tuffnellglass.com
www.flameoff.co.uk

noora

I used powder pink for the ears and nose of my bead trolls (photos posted in the February newbie S&T thread).