what's going on with my Triton beads?

Started by turnedlight, November 30, 2009, 04:07:01 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

turnedlight

 :( I have been using it for ages, and getting the colours I want ie bright and pale blue with a very pearly look - but this week and last it's either not reacting at all or going straight to greys :( boo hoo I'm really sad as it's my favourite..
kathryn

bubblefizz

im no expert- but hows you doing on your gas? could be running low, im sure that would effect it  ::)

turnedlight

That's a thought actually, I'm sure it must be up soon.. how do you know until it actually runs out how much you have left?
I have been doing a little better with the colours this week but still not getting quite the pearl like effect whilst it still being a lovely blue. I was advised it could just be a batch thing too.
kathryn

bubblefizz

you dont really  :o i just have an idea when mines about to run out the flame just goes low verrryyy slowly.
but i remember someone asking that question thats why i thought i would mention it  ;)