Main Menu

Black pearl lookalike

Started by JaySpangles, July 26, 2009, 09:13:21 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

JaySpangles

My mum has some lovely (real) black pearl earrings.  She has asked me to make her a necklace to go with them for her birthday. 
I said that I (obviously) couldn't make her real black pearls, not being an oyster myself, but I would do my best to make something to go with them.  The earrings are a lovely dark grey with a pearlised finish.
Can anyone suggest a starting point please.
As a newbie I haven't enough experience of the attributes of the various types of glass to know where to begin. 
I assume I will have to use a silver glass over a base bead of another colour.   I have a nice dark steel grey transparent effetre, which I think might be nice for spacers, and perhaps a thin layer of something else on top for the main beads???
Any help much appreciated.
Thanks
J x

Veebee

#1
Reichenbach blac reduces to a lovely shine, I can send you a rod to try if you like?



Not the best photo, but might help? I love this glass BTW!
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

Kaz

I am going to make some silvered shards with the last of the black pearl glass some time this week - so PM me your address and I'll send you some to try if you'd like?
This was how it looked on antique clear with some silvered ivory.

Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

SueP

I have some black pearl earrings and necklace and I think dark silver plum is what you want - you can get some shards from Jolene :)

sparrow

Just posting two roses - the first is Dark Silver Plum:



The second is Black Nebula



.......hope it's useful :) And had to laugh at you not being an oyster :)

Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

JaySpangles

I have some dark silver plum, but I haven't succeeded in make it look silvery yet.
It just looks a bit like dark plum (Doh!)
What do I need to do?
Thanks for the offers and suggestions.
I have pm'd.
Many thanks, everybody is so kind and generous on this forum.
J x

flowerjasper

to get the rainbowy colours you need an oxygen rich flame
sandy

Trudi

Quote from: flowerjasper on July 26, 2009, 09:48:23 PM
to get the rainbowy colours you need an oxygen rich flame
sandy


Ohh I've not used it much myself but I would have assumed a propane rich flame ............. just goes to show ya!

clasicat

Quote from: Kaz on July 26, 2009, 09:19:09 PM
I am going to make some silvered shards with the last of the black pearl glass some time this week - so PM me your address and I'll send you some to try if you'd like?
This was how it looked on antique clear with some silvered ivory.

Kazx
WOW  :o Kaz those shards are gorgeous
Claire x