Caution - ASK 104 and silvered stringer

Started by Diane, April 05, 2007, 10:18:19 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Diane

Hi
Thought I'd better pass this on - there's a topic on Wet Canvas where several people seem to be experiencing cracking problems with Ask104 and ivory silvered stringer - I haven't experienced any problems with ASK colours but I  haven't used it with anything other than itself and a little with Effetre.
but I suppose it's better to be aware of any potential problem
Diane

Billie

Definitely worth being aware of. Thanks Diane  :)

astringofbeads

Thanks Diana. I've not had  probs with that but  Ask definitely doesn't like being encased with Lauscha. Anyone tried encasing it with effetre?

Caroline

i didn't think that ASK was suppost to be incased at all

*rowanberry*

I've used SIS with it no problems - but I've heard about the encasing problems though.
Claire

littlegiggles

Apparently the only way to encase ask is to first mix the ask with clear  about 50-50 then use that for the bead then encase... means you have the same colours but it doesnt crack.  I was reading that even with the clear from the same company it misbehaves