Something unexpected with Triton

Started by sublimekate, January 14, 2009, 10:16:18 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

sublimekate

I haven't got a pic to share yet but I thought I'd share this little nugget.

I made a bead ages ago using, amongst other things, triton for surface decoration. It went on my site and bombed, I took it off and it's been lying around since.

Anyway I had the urge to etch stuff today, so popped it in, I thought oh well I'm going to loose the triton effect but never mind, it might look better.

Anyway, when it came out, it hadn't etched where the triton had been, I really wasn't expecting this, and now it's given me loads of ideas, it hasn't kept it's metalic look, it's shiny blue, but endless possiblities me thinks  ;D  ;D  ;D


TiaraHelen

Just started playing with Triton today, Kate, so great timing! Thanks for the tip.
Helen x

Even after all this time, the sun never says to the earth "you owe me".

sparrow

There are a few like that - try some other DH (can't remember which ones, but others might?) But Cirrus CiM also doesn't etch (or only with great difficulty) - great for detail in skies ;)
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

sublimekate

Quote from: sparrow on January 14, 2009, 10:24:53 PM
There are a few like that - try some other DH (can't remember which ones, but others might?) But Cirrus CiM also doesn't etch (or only with great difficulty) - great for detail in skies ;)

Thanks sabine, I've had a rod or two of that lying around, never could thing what to do with it....mmmmmm

Any more colours that don't etch.....anybody????

Vicki

the old terra didn't etch.....if anyone one is lucky enought to still have some...if you have could you send me your address so I can raid your stash with my zorro mask & stripy top  :D :D :D

Lush!

Khaos doesn't etch either - I made this set yonks ago, the black etched and I was really pleased with the contrast.




www.lushlampwork.etsy.com

sublimekate


sparrow

Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Trudi

Gorgeous Julie!!!

I wonder if all/most of the silver rich glass has the same effect!

Carolien

Wow, that really looks cool! Tnx, gonna try that too :)