Can I make marbles from soft glass?

Started by Kimster, December 06, 2013, 11:15:02 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Miriam

I make soft glass marbles all the time. I use boro punties except for the last one, then I use a thin softglass punty. and as said, Drew's book is the book to read.

As for rounding, you could use a normal round mold, but the best tool ever to make round beads is the Infinite Rim Mold!!

You can see some of my marbles at my website: http://www.facet-design.com/wp/fotoalbums/album/72157628635484889/2012-2013-beads.html
groetjes Miriam


Blog | Website | Colorcharts | Glasss

Pat from Canvey

Thanks for posting the link Miriam. I especially like the one with the red flower near the bottom of the group.