redjay

I ordered some yellow on tuffnells and when it arrived it was electric yellow. I noticed on the site that yellow and electric yellow have the same code. I emailed in and the lady said she thought they were the same glass. She was going to get back to me but has not yet.

I am looking for a nice trans yellow that would fit well with a rainbow spectrum of transparent colours. I find the electric yellow just that bit too luminous and bright. Is there another coe104 trans that would fit this criteria?
Thank you in advance.
J

Krysia@No98


there is straw yellow, that's they yellow of striking red before it strikes
-* -  Courage is going from failure to failure with out loosing enthusiasm -*-

Shirley

Mimosa, the lighter one. It's like sherbert lemons. It's streaky, though, rather than solid.
Val Cox Frit - Thai and Bali Silver 

theflyingbedstead

#3
There is also a Lauscha semi-trans yellow - see here http://lauscha.heatherkellyglass.co.uk/content/snt-145-yellow-6-8mm
and an orange-yellow http://lauscha.heatherkellyglass.co.uk/content/snt-151-yellow-orange-6-8mm
If you use them thinly they are more transparent.

Or you could use effetre light amber.
Charlotte x

redjay


Shirley

Don't Effetre do a striking yellow?
Val Cox Frit - Thai and Bali Silver 

cbeadies

I had the same problem when I made some rainbow disc beads a while back, the yellow (Effetre striking yellow) doesn't look quite right and is not as transparent as the other colours either! But it was the best I could find...will be keeping an eye on this thread to see if anyone can suggest a good alternative!