Decals

Started by lddlsa, September 17, 2013, 08:51:35 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

lddlsa

I checked my notes and I had actually pre-fired the coasters and then tack fused the decals at 700 degrees C for 10 minutes but as Zeldazog quite rightly pointed out, my kiln is actually firing hot so maybe I would get a better result at 670 degrees C.  Thank you Trudi, peach would be an interesting colour to try rather than white and thanks Jane C, I have a spare fan and will give it a try :)