Which kiln would you recommend?

Started by The Tartan Trout, June 08, 2013, 06:32:32 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Glyn Burton

I built a vitrograph kiln using a metal bin some old ht10 bricks and bits of kiln shelf. Not very beautiful to look at but it will melt 2 kilos of glass in about one and a half hours. It uses a propane burner from a raku kiln. It would not be too difficult to make one using ceramic fibre blanket and it would be lighter to move around so I think mark 2 will be made like that.