Kugler frits and enamels, any experiences?

Started by noora, December 12, 2012, 08:19:32 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

noora

My local glass dealer has started selling Kugler frits and enamels. She doesn't have photos yet, so I have no idea what they look like. Can anyone share experiences of these, or even photos?

Pauline


noora

Thanks! :-)

Our glass dealer has 1-2 mm frit and 8-11 mm frit. I don't quite know what I would do with the larger one. I wonder, if it's COE 96, can you still pull (thin) stringer and use (sparingly) on COE 104 glass?

Trudi

Hi Noora

Yes you should be able to pull into stringer and use sparingly ... try a few beads to test it out!

Some of the bigger frits are used to pull stringers. I have a kiln with a bead door and I warm them up  in there first before I put near the flame! x