pearl biege and mystic biege

Started by jammie, June 02, 2012, 12:09:48 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

jammie

I've managed to mix up my reichenbach mystic and pearl biege, one is sort of opaque shampooy and one is slightly yellower and clearer, but I dont know which is which, one goes almost cloudy after working, I cant get the shampoo effect properly and think maybe I'm supposed to strike it at the top of the flame, anyone help please? Thankyou!  :)

Lush!

The shampooy one should be pearl beige.  Mystic beige looks more yellow.

And yes, pearl beige does tend to look cloudy rather than pearly when melted  :)


www.lushlampwork.etsy.com

jammie

Ah thanks Julie, I was completely confused! :)