Main Menu

Effetre catalogue

Started by bbpiglet7, July 06, 2011, 04:36:33 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

bbpiglet7

Does anyone know where/if I can get hold of an Effetre rod catalogue please? I know Warm Glass do a Bullseye one but wanted an Effetre also.
Thanks
Liz
x

MadelineBunyan

http://www.effetre.com/murano/prodotti.html

can download and print them yourself (colours might be off), theyre sort of grouped into different booklets of ranges I think.
there were some in the bags at Flame off, but not the full set!

dont know if you can obtain them ready printed.

Lush!

Kaz and I bought a deluxe version at Flame Off auction in 2010 - with rod samples.  Don't know where you could get one of these though, sorry!


www.lushlampwork.etsy.com

cbeadies

Not sure if it's any help, but I printed some pages from here - although printed them a bit small.
http://www.serenasbeadery.com/color-gallery.html

Chris Fisher has a useful characteristics chart of many of the colours.
http://www.chrisfisherart.com/Moretti%20Glass%20Characteristic%20Chart.htm

bbpiglet7

Thanks for the information - found the charts really interesting  :)
Liz
x