New Silver Glass Clio

Started by SuefromYorkshire, March 30, 2010, 02:04:51 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

SuefromYorkshire

Just received my batch of Clio very excited  ;D.
Has anybody had a go with it yet?

If you have any tips for good results they would be very very welcome, as I can be hit and miss with these Silver lovelies! It might be a little premature as I haven't yet tried but I'm about to, let you know how it goes! ;)

helbels

Hi Sue

If you do a search on Clio on the forums there have been a few threads on it already, with some piccies of what people have managed to achieve.

Helen x

SuefromYorkshire

ooh thanks Helen ;D, I've supposed to have looked!  ::)

SuefromYorkshire

Here the are, I'm quite pleased with these ;D, although the big one with the silver in it has a crack! ???


June

Wow, they look pretty good, Sue   ;D  I haven't managed to get much out of it at all as yet!

helbels

I'd love to know your secret Sue, all I've got from mine so far is beige.

SuefromYorkshire

Thank you ladies ;D, first time luck I think, the trick will be repeating them! :D

I just melted them on, not super hot or anything and then flashed them back, after coolin a while, through a small reduced flame (turned down the oxygen, I have a Minor), some of them twice.

They are mostly pure Clio, except the squarish one which is on Striking Red - that's why it's so darker! The very light ones are Clio on Clear.

Good luck, I hope the glass fairies are kind to you! ;D ;D