Main Menu

Reichenbach

Started by SilverGems89, March 21, 2010, 07:24:41 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

SilverGems89

Quote from: Mand on March 22, 2010, 11:36:44 AM
I love Opal Raspberry ;D  Iris Blue is a lovely colour too.

I adooooooore opal raspberry, i bought some the other week and already ordered some more! I got some iris blue at the same time and im starting to think i do something wrong with it cause it goes a really icky green  ???

Veebee

I love Reichenbach, the pearls and mystics are fab, though I think the colours I use most are gold violet, gold ruby bright, and antique clear. The garnet is great too! The black actually bleeds like crazy, completely swallowing anything in it's path, but it also reduces to a lovely silver metallic shine  ;D
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

Pip

I bought some reichenbach 'magic' that's a khaki green colour and is meant to develop oranges, blues etc with working. So far I've managed sludge brown  :-[ - what's the secret?

Veebee

White hot, cool rapidly, gently re-heat.... you should see it "blooming" in the flame!
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

Pip

Thanks so much - I'll try that!

theflyingbedstead

Ocean is VERY beautiful, and Gold Violet is another favourite...more gorgeous, less Barbie than Rubino, and far better behaved! Antique Crystal is another must-have as it works so perfectly with Dirty Martini and Ink Blue. In fact...there are many gorgeous Reichenbach colours, I would recommend getting a sample pack so you can try them all. Martin sells one for £4.00 - such good value!
Charlotte x