Main Menu

Plowden & Thompson glass?

Started by Kalorlo, March 01, 2010, 07:52:05 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

theflyingbedstead

QuoteI use their glass all the time the 93 coe and it fits perfectly with Bullseye.  I teach using the P& T glass
and all my students love it.

That is reassuring to know Pauline. Is it SOOOO much cheaper than Bullseye too. I bought a kilo of clear rods for under a fiver plus VAT, so that is even cheaper than Vetrofond or Effetre.

I really must get some pics of the rods I have and uploaded to the wiki so that everyone can see the lovely colours.
Charlotte x

ejralph

I must admit, I find it just bizarre that they still don't have their own colour chart up online on their website. ::)

I guess business must be very good for them  :D

Emma

Soozintheshed

I taught at Higham Hall last weekend (Fab place - http://www.highamhall.com/)  and used 100 coe P&T, it's a great glass, holds the colour well. 

The Banana Yellow was boiling a bit, was fine for stringers though, the clear is lovely though.  The Caramel is gorgeous.

Here are a few beads I made with it at the class as samples/demos.

The blue is the neon blue, gorgeous colbalty colour..



Sooz     '(0,0)'



www.thebeadshed.co.uk
http://stores.ebay.co.uk/The-Bead-Shed

♥♥Tan♥♥

Lush colours and you do good sample packs of Plowden glass as well don't you SOoz?

Soozintheshed

Sooz     '(0,0)'



www.thebeadshed.co.uk
http://stores.ebay.co.uk/The-Bead-Shed

Kalorlo

Ooh, thanks for posting pics, Sooz!

Hels4444

Great pics Sooz and I did not realise you had sample packs will put it on my shopping list xx

Flyingcheesetoastie

Ooooh a sample pack!  I swear if I get another sample pack my rod shelf will collapse!  i have to actually use some glass up first...

Soozintheshed

Quote from: Flyingcheesetoastie on March 21, 2010, 07:01:48 PM
Ooooh a sample pack!  I swear if I get another sample pack my rod shelf will collapse!  i have to actually use some glass up first...

I keep saying that   ;D
Sooz     '(0,0)'



www.thebeadshed.co.uk
http://stores.ebay.co.uk/The-Bead-Shed