original Terra frit

Started by catriona, July 23, 2009, 05:07:27 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

catriona

I still have quite a lot of this can anyone tell me the best way to work it please ive had it since i first started and forgot about it came across it today .
xxcatxx

turnedlight

Ooh you lucky, lucky..  ;D I would get a clear rod and coat the end in a few dips of terra, and make a thick stringer - terra is very easy, you just reduce a bit, and get lovely colours, or encase for muted lovely colours. It's great on ivory..
kathryn

catriona

Thanks thats great i,ll give that a try i,ve got about 50 grams of it so i,m going to have a great time .

xxcatxx

Dragonfire Glass

Quote from: catriona on July 23, 2009, 08:54:31 PM
Thanks thats great i,ll give that a try i,ve got about 50 grams of it so i,m going to have a great time .

xxcatxx

If you'd like to send a gram or 2 my way, I can be very grateful  ;D

beads-on-toast

i have Terra frit and it is fab
It reacts in a really aggressive way on Dark ivory and sits better with light ivory - if you work in with a marver i have found it produces purples and blues very easily