At What Rate does a Kiln Cool Down?

Started by Stacy, February 19, 2008, 12:47:30 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Stacy

I'm trying to create a excel spreadsheet which will tell me roughly how long a programme will take in my kiln.

I know that it is probably extreamly variable due to different condidtions but does anyone have an idea of an approximate rate that a kiln will cool down when the programme has finished. Or a way that I can calculate it. Is it going to be different on each and every firing? or will it matter how high the kiln is when the programme is done?

I would be more than happy with an approximation...

glassworks

depends on ambient an the kiln.. the bluebird cools naturally at over 100 deg / hour here.. although our internal temp in the barn is only 5 degrees... the xl, which is fire brick lined, cools at less than 40 degree's per hour in the same condition (and should be about the same for an sc2/3, although the sc's with bead doors have a small opening when the door flap is slightly raised... the sc2 cools down slightly faster than the sc3...


Stacy

Thanks hunny!!! xxxxx

Thats exactly what i needed!

Stacy

Now - thanks to my wizzy spreadsheet I know that my pot melt thingy will be ready to come out at about 9:00pm give or take 30 mins or so

Billie


Stacy

Quote from: Billie on February 19, 2008, 01:41:46 PM
Very clever!

you say that now... knowing my luck with excel it will be done at 10am tomorrow morning... ;D

Zeldazog

Oh, I want to do a pot melt thingy!! But I can't in my home kiln, it doesn't go hot enough  :-\

Please post a pic, I will be checking at 9.05 pm!!!

Stacy

Quote from: zeldazog on February 19, 2008, 01:59:16 PM
Oh, I want to do a pot melt thingy!! But I can't in my home kiln, it doesn't go hot enough  :-\

Please post a pic, I will be checking at 9.05 pm!!!

I only have a little kiln so its just a tiny tiny one... it should come out as about 1" in diameter.... i thought that might be a nice size to put a bail on the back of

♥♥Tan♥♥

yay pot melt pot melt, pics please, from every angle and then a few more and how you did it and what you think of it and how hard you found it :D :D :D

Stacy

Well I can tell you now that I used a egg poacher and some mesh you use to fix rusted out old cars... it soooooo professional!  ;D

Stacy

OK - there will be no pictures and we shall never mention the pot melt fiassco again.... :'(

Sal

Oh no! I was really looking forward to finding out what a pot melt is as well! What is it  ???

Zeldazog

Why, what happened, Stacy? You can't leave us hanging on like that!

Stacy

errrrr.... it melted..... along with the egg poacher and mesh thingy that I rigged up

Its all one sort of metal and glass blob....in the future when I am a world renowed glass artist I think I will call this my industrial era.

Going to have another go at the end of the week when I have rigged up something a little more unmeltable!

Stacy

Quote from: Sal on February 19, 2008, 07:15:31 PM
Oh no! I was really looking forward to finding out what a pot melt is as well! What is it  ???

Its when you put a load of glass ontop of a wire mesh or pot with holes in it. You pop it in the kiln and the glass melts through the holes into a puddle on the kiln shelf - you put lots of different colours in and they all swirl together.

Well that was my interpretation anyway - but we know how that ended!  ;D