Not sure if any ones spotted this before but its a short online movie of the Kiln being progammed for the variety of ramps for annealing glass.

http://www.paragonweb.com/VideoInfo.cfm?VID=2

glassworks


Lyn G

Ray,

Thanks so much for displaying that link - it has all become clear now!!  I have only been using my kiln for just over a week now and haven't programmed it at all.....apart from getting it to switch itself off about half an hour or so after I have finished for the evening.  No broken beads yet!!  :D

Anyway, after watching this I will definitely have a go!!

Thanks again.

Lyn

Kaz

Oh thanks for that - I have not started using my kiln yet and this is really helpful! Also the video on shelfwashing too!
Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!