cromartie electric hobby kiln

Started by sandmor1, March 05, 2014, 08:46:34 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Jane C ♫

There's sample firing schedules on manufacturers websites, so no need to buy software.

Good call about not getting the pottery kiln - I have an old cromartie (for pottery, not glass) and found out it would cost about £500 to convert it to digital (and the old style fibre lids aren't replaceable so no point in wasting the money).

Enjoy!
Hand Painted Silk and Fused Glass Artist.