theflyingbedstead

I have got a coppery colour lustre when gold fuming over Thompsons black enamel (which Tuffnells sell).

You can then etch patterns by using a mask over the lustre that you want to keep and dipping the bead for 4 seconds in etch-all liquid. I use a mask made of nail varnish or masking tape or vinyl.  ;D
Charlotte x