Main Menu

Tube for baubles

Started by SilverGems89, November 20, 2013, 01:06:19 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

SilverGems89

Hi everyone! I am feeling like being brave and having a go at blowing some baubles for Xmas, what tube would be the best size? And wall thickness?

Marcel

It depends a bit what your set up is  ;)
are you on tank or concentrator?
i use 24 mm wall thicknes 2,5 mm on concentrators i use
a bethlehem Alpha for that
and i use 30 mm wallthickness 2,8 on my bravo  8) and that is on tank

SilverGems89

I've got an Alpha on a concentrator  ;D I'm torn between 18mm/2.5mm wall, 24mm/1.8mm wall or 24mm/2.5mm wall  :-\

garishglobes

I use 32mm with a 4mm wall thickness but have a big torch and a couple of large concentrators.

With a smaller set-up, I'd be tempted to go with either 24mm and 1.8mm-2.5mm wall or 18mm and 1.8mm wall. The size of tube will determine the size of the bauble to an extent.

I don't think it'll matter too much which you go for - I'm assuming the concentrator is 10l? If not, then I think I'd be tempted to go with the 1.8mm wall. The 1.8mm will melt a bit quicker so you'll lose on the control front but set against that, you'll gain because it'll soften quicker if you have less heat, if that makes sense.


Lotti

Quote from: garishglobes on November 20, 2013, 07:43:27 PM
I use 32mm with a 4mm wall thickness but have a big torch and a couple of large concentrators.

With a smaller set-up, I'd be tempted to go with either 24mm and 1.8mm-2.5mm wall or 18mm and 1.8mm wall. The size of tube will determine the size of the bauble to an extent.

I don't think it'll matter too much which you go for - I'm assuming the concentrator is 10l? If not, then I think I'd be tempted to go with the 1.8mm wall. The 1.8mm will melt a bit quicker so you'll lose on the control front but set against that, you'll gain because it'll soften quicker if you have less heat, if that makes sense.



I have the 18 with a 1.8 wall.  ;) :)

SilverGems89

Thanks everyone, I think I will go with the 1.8mm wall thickness, will ponder the diameter a bit more  :)