Started by lemon kitten, October 23, 2013, 08:15:47 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

lemon kitten

How on earth do I split my beads in half for slumping?  I've tried using a metal punch to split down the hole but the entire bead just breaks.......any suggestions please?

Janey
Never stand up in a canoe!

qwirkyglass

mine do it on thier own when i let them get too cold before putting them in bubbles.
do you cool in bubbles or kiln? :)

lemon kitten

No I anneal in the kiln.....but I do sometimes want to use beads that haven't quite turned out the way I want.  I never purposely make beads to slump

J x
Never stand up in a canoe!

julieHB

I filed the point of a round nail so that it had two opposite sharp edges, and when the point is inserted into the bead hole only the edges touch the glass. Then, with confidence (!), I hit the nail with a hammer. After some practice you'll end up with two halves - they might not be exactly equal in size, but pretty close. This works best with beads that are equally thick around the circumference. For lentils and similar I suggest melting them down as they are, or optionally grind one side flat before fusing.

Julie xx