Main Menu

Torch

Started by Lotti, October 18, 2013, 01:06:14 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

tinker

Thanks for this really informative post, I've been wanting to play with boro too :)

Does anyone have any experience or advice with regards to working it on a cricket? I plan to get another oxy in the new year but wasn't really sure whether I need to hold out for a bigger torch too or whether I'd be content for the time being on the cricket.

jammie

#16
Tan did a post (not sure where though) of working boro on one oxy, I can manage 9mm rods on a bobcat and one oxy so think you would be ok ! but that is only clear, haven't tried colour yet. Just waiting for xmas to order some clear from Sean!  :)
My bobcat is still giving me a reducing flame and am struggling to get the oxy to give out enough, some seem to have more output than others is that possible? I was going for another oxycon but didn't have enough money when it came to it so will just ave to ait and make do with what I have for now.

Steampunkglass

Quote from: jammie on October 20, 2013, 05:56:41 PM
My bobcat is still giving me a reducing flame and am struggling to get the oxy to give out enough, some seem to have more output than others is that possible?
I knew that the oldest one of my two oxys was on the way out when I got more of a reducing atmosphere as the day's work went on, even though the dial was still saying it was producing enough pressure after a few hours anything with turbo cobalt was going ashy grey. If it's old perhaps it's not producing as pure an oxygen output anymore?  ??? ??? ???

jammie

It was 2nd hand but fine when I bought it, its the white and blues and pinks and anything that can go metallic. I thought another oxy would sort it and i could do more boro too, sadly my bankie was empty! :)

liquidglass

Quote from: jammie on October 20, 2013, 05:56:41 PM
Tan did a post (not sure where though) of working boro on one oxy, I can manage 9mm rods on a bobcat and one oxy so think you would be ok ! but that is only clear, haven't tried colour yet. Just waiting for xmas to order some clear from Sean!  :)
My bobcat is still giving me a reducing flame and am struggling to get the oxy to give out enough, some seem to have more output than others is that possible? I was going for another oxycon but didn't have enough money when it came to it so will just ave to ait and make do with what I have for now.

Just a quick note:

Tan's post for working on one oxycon is here - http://www.meltinglass.co.uk/article.php?xArt=8