Basic glass cutting for fusing - short video tutorials

Started by handmadeheaven.biz, January 11, 2007, 01:50:06 PM

Previous topic - Next topic

0 Members and 3 Guests are viewing this topic.

handmadeheaven.biz

VIDEO ONE: Scoring and breaking glass freehand


that's just for bigger pieces tho. For small pieces...

VIDEO TWO: Cutting and breaking smaller pieces of glass with breaking pliers

♥♥Tan♥♥

AAhhh breaking pliers, I didnt know such a thing existed, no more slashed fingers when breaking small bits then

handmadeheaven.biz

the rubber coated metal ones are ones i normally use as they have a spring to make them easy to use and they dont scratch the glass, but i recently bought the cheaper plastic ones for small, fiddly bits

BeadyBugs

How were the plastic ones Steph?  Any better on fiddly bits?

HP x
Helen P

handmadeheaven.biz

yeah, they were better. they have a raised plastic line which runs along the cut & works better than the rubberised ones. they have a C shape which works well for bigger pieces but not on tiny ones. they were worth the ?3 or whatever they were. tho i wish they had a spring...