Can I use stainless steel rod rest in kiln?

Started by Kimster, June 02, 2012, 06:01:46 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Kimster

Quick question...these things always seem to arise when the suppliers are shut! I have one of those £5 rod rests...I bought it at Flame Off from either Tuffnells or Off Mandrel..Would it be OK in kiln on either garaging/batch annealing prog? I'm on a roll here! & could do with putting another 20 or so in, just don't want to lie them on top of others if I can avoid it  :-\ Thanks all - aren't 4 day bank holidays fantastic  :D  :D

flame n fuse

stainless steel should be OK - that's what mandrels are made of. Have fun!

Kimster

Thank you Flame n fuse :) .. just occupied myself making silvered stringers while I waited for a reply! Do you happen to know if I can anneal Lauscha glass at soak temp of 520 c ? I think I read somewhere on the forum it needs a higher temp but I have no idea how to go 'off pre programmed' as it were!

Shirley

You should be fine with the stand in the kiln.

Lauscha anneals the same as the other 104 glass - Effetre, Reichenbach and so on. It's common to mix it with other glasses anyway :)
Val Cox Frit - Thai and Bali Silver 

Kimster

Thanks Shirley! Just seen some lovely Lauscha Cocoa / copper green beads & would love to give them a go  :)

Shirley

Val Cox Frit - Thai and Bali Silver 

Redhotsal

Your rod rest will be fine but just be aware that it will probably go black! My experience with Lauscha is that to anneal it properly you do need to go higher and longer in temperature. I'd always heard that but I don't actually know what the perameters are. I only know that when I annealed Lauscha clear on a 520 Effetre cycle once it didn't appear fully annealed with polarisers.  :-\

Kimster

Oh...thanks Sally. I think I'll give it a go on the normal 520 cycle, since  these first efforts are only for me. I'll see if I can find some instructions to do a hotter cycle once I know what I'm doing  ;D

Redhotsal

It should be okay - let's face it - a slow ramp down in temperature is going to be better than no ramp down. I've had a look at Heather's website, where she has an annealing schedule. The temperature is a little higher but it would appear that the critical difference between an Effetre anneal and a Lauscha anneal is that the Lauscha seems to require more time: http://lauscha.heatherkellyglass.co.uk/content/annealing-schedule

Kimster

Thanks Sally, that's really useful. Looks like I can get away with the normal garaging prog, as long as I make the Lauscha ones first to ensure the longer cooking time  :)