Making a cab on the end of a mandrel

Started by Donna@Rockin' Beads, May 31, 2012, 08:21:43 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Donna@Rockin' Beads

What size mandrel do you guys use to make a cab on?
I have a cab mandrel but fancy trying to make one 'Patti Walton' style (at the Flame Off this year). I've tried a 5mm and the bead release fell off before I even got started (too cool, I guess) and a 2mm - managed an ok cab at the end but it was wobbling furiously by the time I plonked it onto the bottom of the kiln  ;D
So, for those of you that do...... What size and any tips?
Thanks guys  ;D

sparrow

I usually make them on 2mm mandrels....but not as big as Pati!  ;D
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Margram

Yes, 2mm - and keep warming the back! :)
Marg x  Etsy Flickr My blog

julieHB

I almost always use 2.4mm - just a tad sturdier than the 2mm, but not so big that it draws the heat out of the glass to quickly.
Julie xx

                           My Webbie - My Flickr

MangoBeads

Any size but the bigger the mandrel anchor the glass further down the tip so more of the mandrel is inside the cab . Does that makes sense ?

mizgeorge

Julie's beadspanner makes these a whole lot easier too!

Donna@Rockin' Beads

Excellent. So, really I just need to practise  ;D
Your bead spanner looks great Julie, maybe you'd like me to stock it in the shop for you  ;D ;D

Krysia@No98


Maybe look at your bead release too, is it too thick?
-* -  Courage is going from failure to failure with out loosing enthusiasm -*-

SilverGems89

I use 2.4mm mandrels for cabs also, if it's wobbling your working too hot  :P

Donna@Rockin' Beads

I dont think it was wobbling because it was too hot. I think I wasn't quite gentle enough  :)

SilverGems89

Quote from: Donna@Rockin' Beads on May 31, 2012, 07:16:10 PM
I dont think it was wobbling because it was too hot. I think I wasn't quite gentle enough  :)

ahhhhh, yeah, i always use fresh dipped and flame dried mandrels for cabs  ;D

Donna@Rockin' Beads


JKC

I use 1.6 mandrel for stud earrings. Janet

Lush!

I like big ones ... mandrels, that is  ;D


www.lushlampwork.etsy.com

Diane

QuoteI like big ones ... mandrels, that is

Well someone had to lower the tone ::) ;D ;D ;D