Oooh, new kiln arrived, do I need fibre paper?

Started by Kimster, May 24, 2012, 03:22:51 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Kimster

Beside myself with excitement &  can't wait to have a go with my Kilncare Ace! Just read the instructions & it says use fibre paper to put my beads on....where do you recommend I get this from & do I definitely need it? Any advice welcome as usual (just noticed I have 2 stars & am not a newbie any more..that is so not true! How did that happen? Don't want to be 'promoted' up with the big girls before my time!!)

Donna@Rockin' Beads

I have a wire mesh which I poke the mandrels into. On the base of the mesh I have a fibre blanket pad thing that came with my kiln.
The mesh is easy to shape and will keep your beads off the base of the kiln but some sort of protection is recommended anyway in case of melting incidents (never had one, phew).

poledra1958

I think if you are batch annealing then a lot of people just pile the beads in a dish.

If you are garaging then you can get a mandrel rest for the kiln from Tuffnells  (woud think the one for the SG2 will fit)

As for the stars the more you post the more stars you get  ;D ;D ;D ;D

HH on Bulk,

Kimster

Quote from: poledra1958 on May 24, 2012, 03:51:17 PM
I think if you are batch annealing then a lot of people just pile the beads in a dish.


Thanks Jenny. Another dumb question, what should the dish be made out of ?!  ::)

Krysia@No98


No need for fiberpaper for beads, if you are going to do slumping in there then you will need fiberpaper bla bla bla  :)

Because when the beads go in the kiln they will not be melty they will be in solid form.

Quote from: Kimster on May 24, 2012, 04:48:25 PM

Thanks Jenny. Another dumb question, what should the dish be made out of ?!  ::)

a pirex dish from wilkos will be fine, nothing fancy

-* -  Courage is going from failure to failure with out loosing enthusiasm -*-

Les

I think some folk use plain old terracotta dishes :)

Les


Krysia@No98

-* -  Courage is going from failure to failure with out loosing enthusiasm -*-

Pat from Canvey

If you want to be super careful, a plain white tile will do on the bottom of the kiln.

SilverGems89

These are all just precautions, if something goes wrong and the temperature gets too high and your beads melt into a big puddle they wont stick and ruin your shelf, so no you don't necessarily need fibre paper (which is quite expensive) any of the other suggestions in this thread will be just as good (and probably cheaper!)

fionaess

I use an old pyrex bowl for my soft glass beads


If it's got a hole, it's a bead !

Kimster

Ready to have a go now - gawd - just to check, I have 89 beads all piled up in a glass bowl which I hope is pyrex! Is it OK that they're all on top of each other & touching each other?  ???  ???

spexy

Can I add a word of caution. I batch annealed all the beads I had been making from when I started, a big pile in a pyrex bowl and they all stuck together. I had a lot of beads with Rubino and some Iris orange which broke into bits. I did have the correct temperature settings.

I would do them kebab style on short mandrels.

BeeBeads

I do the same as Linda Spexy, on short mandrels - great for using up your bent and mangled ones!
I've never tried the Pyrex bowl method so can't comment.
And I use kiln shelf paper on the shelf and the floor of the kiln, just as a precaution  ;)
I'm still using the huge sheet that I bought with the kiln, years ago.  Just cut it to size and you can use it for more
than one firing so it's not as expensive as you think.

Best of luck, the first firing is very exciting!

fionaess

#14
Quote from: spexy on May 25, 2012, 08:52:48 AM
Can I add a word of caution. I batch annealed all the beads I had been making from when I started, a big pile in a pyrex bowl and they all stuck together. I had a lot of beads with Rubino and some Iris orange which broke into bits. I did have the correct temperature settings.

I would do them kebab style on short mandrels.

Unusual - I've batch annealed for about 5 years now, used the same pyrex bowl and never had this happen... ???


If it's got a hole, it's a bead !