Picking your brains really. I am fine with making the ring toppers and cabs that are similar to Manda's/Carla's and the way to encase them, however, I am trying to find the best way of encasing a colour in clear on a topper or cab. What I mean is when you make a core of a colour and encase it in clear - like you would a bead. I am trying to find a way that ensures that there are as few bubbles as possible and that the core bit looks central. I am having reasonable success with the three ways I have tried so far - trying to get a big enough blob of clear to cover the whole thing in one swoop (fairly successful but challenging), trying to do it like encasing a bead and bringing the clear together by tilting it forward (works but sometimes results in an air bubble in the centre) and trying to build it up by adding a blob to the top and then gradually working towards the back with rings of clear that are added to the right of the edge of the previous clear (IYKWIM) (least successful).
I'd be interested in hearing any other methods that work well for you!
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

sarah t

 limited experice but the large blob on top in the middle and then melt/ tilt /roll and add to the edges when needed was the combination i went for


MangoBeads

I use the same way as Julie HB .... big blob then push it from the top and down the edges ...Julie has a more technical term for it but I will let her use her special terminology :) ...enables a thin even encasing layer ...I'm sure she will be along to add to it :)

Chameleon

I do pretty much the same, I heat a reasonable size gather, place it on the centre of the cab, then i apply a little extra heat to the clear before turning it upside down and pushing it into a lentil press / marble roller / whatever is to hand  :)

chipperpottery

Same here, only I do need to remember to leave enough area for the clear, onlI end up that they are to big for the press  ::)

ScarletLeonard

Personally I've found for a full encasement it easier to build a ring of clear first enough to nearly cover the colour. Add the blob of colour in the middle then a small blob of clear on top of the colour then melt it all in. That was on the hothead though and any other attempts at encasing resulted in cracks on the toppers for me.

Trouble with that method though is you are pretty much limited on what you can do decoration wise it's pretty much frit or foil or nothing.

Lush!

I think my method is probably the same as others have said, but I do it like making a shank button.  I melt a really big gather of clear, hold the mandrel straight upright, at 90 degrees to the table top, and drop the gather onto the centre of the topper.  Then give loads of heat to the clear so that it melts down gently, whilst constantly turning (in the normal horizontal position).  I don't press or touch it with tools until there's absolutely no undercut between the clear and glass underneath.


www.lushlampwork.etsy.com

Jennie Lamb

I learnt from Julie HB the Rocking method!?  Very good for thin encasing!!

awrylemming


julieHB

Manda and Jennie, I believe the technical term is wiggle-woggle....or was it wibble-wobble??  ;D ;D I believe the "rocking method" is a much more precise description! ::)

I most often encase my cabs, up to three times, so I needed to find a method to make thin and even layers. Same as many here, I centre a blob of glass on the top of the cab core, then heat the blob without melting the core, press flat with a marver and "wiggle-woggle" in one direction, then 90 degrees to it. Then I direct the heat on the encasement edges only, by pointing the mandrel towards me from about 10 o'clock, and marver down towards the edge, working my way round and round the cab until the whole cab is encased.

With heat control you can encase the whole cab without distorting the core at all. You end up with a cab that has no "window" along the outer edge.

There's another way which I have only experimented with (and with results ranging from fantastic to disastrous  ;D ) Melt an appropriate sized blob of the encasing glass and squish to a paddle. Make your cab base, and after pre-warming the paddle touch it to the centre of the cab and gently melt and marver it it onto the cab. Makes for a very even, thin layer, and with no distortion to the core at all. That's the theory, anyway   ::)

If i want a thick encasing I use the "around the world" method, starting from the centre. It can, as with beads, trap bubbles, but with practise it won't.
Julie xx

                           My Webbie - My Flickr

Kaz

Thanks all! Lots more ways to try now!!! Never thought about round the wold from the centre backwards, as I usually encase left to right! Will give that a whirl too!!
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!