Main Menu

Shaping beads

Started by Hazer, December 16, 2011, 09:08:37 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Hazer

Out of interest (and not because I typically spend 30 mins shaping one small bead), how long do you spend shaping a bead (without a roller/press)?

I'm finding that getting symmetry on mashed beads in particular is really time-consuming!
ContinuumDesigns- artisan polymer clay beads for one-of-a-kind designs.

The FHFTeam - featuring glass, jewellery and art handmade in the UK.

awrylemming

About 3 - 5 minutes I think.  I generally make a tube bead to mash, and then put a couple of rounds of glass in the centre to get a bicone-ish shape, and then mash it.  It should be about right and not need any faffing after.