Main Menu

lessons or torch ?

Started by Sheena, September 24, 2011, 09:19:50 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Sheena

Hi,
I'm on a hot head on bulk fuel but now want to move up to a duel fuel BUT I'm also at the stage where I need some intermediate lessons to get the best ot of DH glass, consistancy, shaping etc...... As I live in Ireland when I add up the cost of Flying over to UK, trains, accomodation and lessons it's coming to same price as torch and oxycon!
So being experienced bead makers what would you suggest?
1, Get lessons and stick with the hothead for a while longer (but will get frustrated if I have the know-how but not tools)
2, Get torch (but will get frustrated with cool equipment if I don't really know how to use it to get the best results)

Any sugestions appreciated....
Sheena

Dee Dee

Personally, I would get the torch, Sheena!  Just having a dual fuel torch would widen your abilities, and get you closer to getting the best out DH glass and shaping etc!

GaysieMay

I would also get the torch first, you will learn how your new flame reacts in readiness for lessons in the future, as most teachers will have duel fuel set ups.  :)
www.GaysieMay.etsy.com
www.facebook.com/gaysiemay

garishglobes

I'd agree. Go for the torch - the dual fuel set up may well help with some of the DH glass. And do lots of reading about the glasses and so on, and how they might work with that new torch :)

squirsygirl

torch - you'll see a massive difference straight away.  Plus there's masses of info and advice on FH!

Kirsty

The Tartan Trout


TracyJayne


Mand

Get torch and play.  Buy some e-tutorials? Much cheaper than flights and lessons. ;) 

I'm pleased with my Nortel Minor.   Very easy to use.  ;)

paintboxcrafts

Torch, torch, torch, torch, torch!
Imagine having lessons on a lovely dual fuel set up and having to go back to your hot head!
www.paintboxcrafts.co.uk  www.paintboxcrafts.etsy.com

Madam Steph

The torch first.
I've had my GTT Cricket a couple of months now and it's so much more versatile.
I have my first lesson booked for beginning of November, so it's all practice time 'tween now and then

Magpie

Another vote for torch. Coz otherwise you'll 'waste' the first half of your lesson getting used to the dual fuel torch you're being taught on. Get used to it and save, then do lessons.

Fruddy

Another vote for the Torch!!

I think that the best way to learn about glass is just to play and practice with it... as others have said, get a couple of Tuts (Anouk's Tutorials on how to make Silver Glass sing are brilliant) and just have fun!

Chameleon

Id vote torch too  :) 

just in case you havent seen them there are always EOM Workshops in Ireland, they have some great classes

Fiona


Corinne Lacy

Hi, are you the Sheena I took to Milton Keynes station after Flame Off this year???

I've now got a Nortel Minor, oxycon and extraction system from Tuffnells without having any more tuition and love it! I would say get the new torch set up then practice, practice, practice.....then get lessons later on. They will make much more sense having got to know your torch first. You won't forget anything from your tuition cos you will be able to go back to your torch straight away.

Are you coming to flame off next year?? If you need any help with transport again don't hesitate to ask  ;D

Corinne x