Main Menu

May Boro Test Recipies

Started by stuwaudby, May 29, 2011, 12:42:20 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Chameleon

You've got some gorgeous colours there, lovely beads all of them  :) I think 7 is the non boro ones

stuwaudby

No one has guessed it yet. Keep trying.

Hazel

Is it no 10?
I love no 8 - looks like dichro in there
Hazel

stuwaudby

I give up on you lot...

Set 9 is Not Boro.

Set 9 is made using a Reichenbach multi / effetre twistie and encased in effetre (some are Laucha encased). Flame strike and annealed at 520 for a bit more purple. Some are multi twisted over black and some multi over amethyst.

Lyn G

I was just about to say Set 9.....it's obvious really!   ;) ;)


JKC

They are all lovely boro or not, I couldn't decide which set were not boro.