What's going on here then?

Started by Amber, April 27, 2011, 12:44:43 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Amber



Loads of my etched beads have developed this white gunk around the bead holes and I'm really worried about the ones I've sold now... :-\

What is it and can I get rid of it?

ARBeads

Not seen that before, are you remembering to neutralise the etching fluid in a solution of Bicarb/water and then a really good rinse in plain water?

Just a thought x
Ruth & Andy


www.etsy.com/shop/arjewellery for beads!

Josephine

I agree, neutralise and then give them a gentle scrub with an old toothbrush and a tiny bit of washing up liquid in warm water.

Les

I use an old toothbrush too. It works a treat :)

ScarletLeonard

ahhh bicarb and water.... thats what I was doing wrong, I get that gunk around the dots.

Magpie

Quote from: Josephine on April 27, 2011, 01:10:36 PM
..... a gentle scrub with an old toothbrush ......
Quote from: Lesley Jane on April 27, 2011, 01:13:40 PM
I use an old toothbrush too.

So was it wrong to use D's toothbrush? He hadn't done anything to annoy me, but there were only two toothbrushes and there was no way I'd use mine! Should I have used toothpaste to scrub with or was the soap OK? He didn't say it tasted funny or anything......

::)