Cleaning annealing bubble

Started by Lotti, April 26, 2011, 10:52:08 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Lotti

I think, no I know that I have got tiny bits of bead release in my annealing bubble and wonder how I can clean this, I was thinking of putting the annealing bubble in a sieve and washing it and hoping that the bead release will disolve or is there a better way.  I keep getting little faults on the surface of beads in annealing bubble and wonder if it might be due little specs of bead release sticking to the warm bead? :)

helbels

If you are getting little dot indentations on your beads it's because you are putting your bead into the annealing bubbles too hot, and the bubbles themselves are sticking to the surface of the bead.  Try waiting until the glow has completely gone before placing your beads in the bubbles x

MangoBeads

Give it a shake Lotti so the bead release will move to the bottom .... the indentations will be due to the beads being a bit to warn when you put them in.
Dont wash them they will just crumble even more :0)