Hiya

I'm periodically tempted by buying a bead liner, but to be honest, all this talk of having to anneal silver tubing puts me right off.  I have a tiny work area, and no real room to store lots of tools etc, and it all sounds a bit of a pallaver tbh.

Anyone want to persuade me otherwise?

MangoBeads

It's no problem you only need a small torch and a cup of water takes seconds , don't let that put you off !

helenfc

Its fine, doesnt take long at all, you could just get a wee kitchen creme brulee type torch for it, they are cheap and easy to refill :)

Redhotsal

Well, yes, I agree with the above - but you'll also have to pickle your silver too because when you heat it up it'll go black. You can get safety pickle from Cooksons etc. or I used to pickle mine in slightly warm Cilit Bang, which seemed to work quite well.

turnedlight

Ooh, good tip - I am just about out of my pickle from cooksons! ;D
kathryn

Kaz

I buy the pre-annealed stuff from Ginko or the thin wall from rashbels and do no annealing or pickling at all!
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

noora

If you have a kiln you can anneal silver in the kiln :-) The annealing temperature of sterling silver is between 600-650 C and you only have to heat it for a few minutes. I find kiln annealing of silver to be much easier than annealing with a torch, since you don't risk overdoing it and melting the silver.

You still have to pickle it to remove the tarnish and most likely brush/polish it as silver often goes a bit matte when you heat it.

Blue Box Studio

Quote from: MangoBeads on April 13, 2011, 06:37:07 PM
It's no problem you only need a small torch and a cup of water takes seconds , don't let that put you off !

You need a soft cushion on the floor to kneel on as well - or isn't hiding under a cupboard a necessary part?  ;)  ;)  ;)
Sue
Website ~ Etsy ~ Blog ~ Flickr

MangoBeads