can i ask a question about bead release?

Started by lejjewellery, March 04, 2011, 02:22:38 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

lejjewellery

I have been lampworking for about 8-9 months now and i usually get the small pots of bead release from martin however when i ordered from off mandrel i got a big tub of bead release and was quite worried to read it contained a chemical which is known to cause cancer when in the air.
Is this the same for all bead release? are the 2 pots i use the same? is it something you worry about?
I do get a bit of breakage on the bead release when i am pressing etc so it has just worried me abit and i thought i would ask.

★★Terri★★

Bead release contains silica - and this if allowed to get into the air as fine particles can cause health problems.

The best way to deal with it is to prevent dust and keep it damp. 

That is don't allow dribbles to dry on on the pot or around the rim and then scrap them - wash them off with a damp sponge.

Any bead release dust and crumbs that get on your work bench - clean up with a damp sponge

Before you try to get your beads off the mandrels dip them in water - then any release cracking off should not form dust.

Obviously the release on the mandrel needs to be dry to make beads, but as long as you keep from making dust you should be fine.

Oh, and if you get it on your hands - then wash it off rather than just wiping them on a towel or tissue.



But, yes the small pots and the big pots, no matter where you get them from, will contain silica.

mizgeorge

I think it's just a case that you've got a new pot with an international label - which features the mandatory Californian Proposition 65 notice. Which seems to include virtually every substance you can imagine!!

lejjewellery

Thank you both, sorry never got back sooner but i went away for the weekend  ;D.

Princess Peggy (Priscilla McGirr)

I worked for 30 years as a potter and must have breathed in tons of dust from the clay..(before the days of Health and Safety), so although it can be harmful, and some miners have suffered devastating silicosis from their years of work, I really don't think it is something that we should worry about unduly, as long as we treat it sensibly, like using the bead reamer in water, and wiping down with a damp cloth after using it.  Silica isn't an instant poison, in fact I would be more worried about the aluminium content, but that's just my opinion.
Pris
My Website http://www.dancingwithglass.co.uk  My Etsy http://www.etsy.com/shop/princesspeggy01
My Facebook page: https://www.facebook.com/DancingwithglassLampwork

Hamilton Taylor

Silica dust can cause silicosis - a very nasty lung condition. But, you need to be exposed to high levels of fine, airborne dust for many years to put yourself at serious risk, and the threat posed by bead release is minimal. Far, far less than, say, lying on a sandy beach breathing the dust being constantly kicked up be people all around you....

The warnings are there because legislation says that they need to be there, when the substance involved is an ingredient. There is little sensible treatment of exposure levels. But, it's still good practice to treat bead release 'wet' at all stages of the process where this is possible.

Regards,

Sean