Started by Lush!, February 15, 2011, 01:21:52 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Lush!

Let's see your beads made with Helios, the lovely new glass from Double Helix.

I  had a couple of rods to test and I found it such an easy glass to get on with, I made loads of beads with just over one rod.  I already showed these but to get the ball rolling in this thread, here's a couple of my favourites again.


Helios Heart by LushLampwork, on Flickr


Helios Big Hole Bead by LushLampwork, on Flickr

Also, more pics and thoughts from me in my blog post http://juliefountain.blogspot.com/2011/02/testing-helios-and-marine-wave.html

Now show us yours - and tell us how!


www.lushlampwork.etsy.com

Diane

Couldn't agree more Dean - that put me off a bit - but not for long ;D ;D ;D
Diane x

Ness

Ah rats - I forgot to try Helios on Helios,  but if i remember next time, I will (thanks Vicki).  I don't have any Dark Matter, but look forward to someone showing some beads... ;)

These are the results of my quick play yesterday -  (not great pics, sorry)



From l-r 
simple Helios spacer;
Helios with a light reduction and wrap of stringer;
Helios heavily reduced, taken back to amber, reduced again and wrap of clear, melted in.  This bead has a really lovely opalescence where it reflects the shine from the inside of the bead.
Next one (the milky one)  bit more reduction than the little Saturn bead and encased.  It's nicer IRL, like a milky opal. 
Lastly black with silver and Helios,reduced and encased.  It's very shiny and opalescent.

When I was playing I wasn't sure I liked it, but looking at the beads I can think of more combinations I'd like to try.  Not sure it's worth encasing it when there are so many silver glasses that love to be encased.


Pam

Here are some sample beads I made with Aion yonks ago.
Sorry about the poor photo, the light is so bad here today.


MangoBeads


All of these use Helios as surface decoration not very consistant results i'm afraid  :) but I do love the glass ;D

IMG_7861 by Mangobeads, on Flickr
IMG_7855 by Mangobeads, on Flickr
IMG_7882 by Mangobeads, on Flickr
IMG_7878 by Mangobeads, on Flickr
IMG_7854 by Mangobeads, on Flickr
IMG_7864 by Mangobeads, on Flickr

Veebee

Good grief Manda, they are stunning  :o

Thought I would show proof of my observations, nothing changed in the kiln ( I batch anneal):

The dots are Helios, honest, and you can see the blue/turqoise (bottom right) where the Dark Matter was fumed:



And this dreadful photo  ::) is very lightly reduced Helios dots on top of heavily reduced (but still gold, not silver) Helios:



You can see the purpley blue which has proved rather difficult to photograph...
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

Veebee

From playing last weekend:

Had a go at Sarah Hornik tutorial, love the pinky orange on the Helios


same tutorial, but the Helios went blue!?


and a weird one, lost some of the shine in the kiln  :(