Coring Beads.... Aaarrrghhh!

Started by Fruddy, January 14, 2011, 10:13:11 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Fruddy

Okay, so  have spent the best part of this evening, coring beads that I am not really bothered about - they're okay - but I wouldn't sell them - with copper tubing.  cos its cheap, and I don't care if I ruin it, or the bead in the process.

After about 2 manky starts, I have managed to successfully core 4 beads.  Excellent!!

So.

There's one bead that I am REALLY pleased with.  Perfect in shape and size, made with a black base and then layered with DH Gaia, with Aurae poked dots.  Twas a lovely bead.

I cut myself a piece of silver, exactly the right size.  Set it into the bead and set about flaring it in my press.  No probs!

My Jim Moore has two stages.  First, you use the large metal die and anvil to flare the silver, then, swap this for the narrower die to press into the bead and finally, swap the metal die and anvil for plastic ones, which "press" the silver into the sides of the bead, for a perfect fit.  I hasten to add that this process had worked 100% fine in the copper cored manky beads that I had practiced on earlier in the evening.

Everything went fine, until I swapped the steel anvil and die for the plastic ones.  Finishing touches, but as soon as I pressed down......

The BL*ODY BEAD BROKE!!

Could have cried.

Have come in, in disgust.

All that practising with beads that I don't give a monkeys about and then, with the one that I actually WANTED to core, the damn thing breaks!!

Oh well.

There's always tomorrow.

;D

Off to bed now.

Peed off.

Margram

Marg x  Etsy Flickr My blog

julieHB

It's happened to all of us - better luck tomorrow!!  :)
Julie xx

                           My Webbie - My Flickr

JKC

That's a shame, but I'm sure the effort will be worth it in the end.

paintboxcrafts

That's pants. Did you anneal your silver first?
www.paintboxcrafts.co.uk  www.paintboxcrafts.etsy.com

MangoBeads

oh no !!! in my early days I only successfully cored 5 out of 10 beads a week ! Hope that makes you feel better .... and I still break a few :) Dont give up perseverance WILL reap reward !

Shirl

Oh what a pain!

I am not even going to attempt it as it seems so difficult