The Tartan Trout

Could you please tell me what I'm doing wrong. I have just tried out some double helix. The striking ones have worked well and look lovely. When it comes to reduction, not so well. They are going black ( like soot) I turn the O2 back up and it burns it off. Is this right or am I doing it all wrong. The colours are popping, but I'm just not convinced.
Thank you in anticipation :) x

Kalorlo

You might be over-reducing them if you're getting a coating of soot. It depends on the colour, but you mostly don't need to turn the oxy all the way off. Turn it down (or the propane up) so you get long yellow candles, then wave your bead back and forth through the flame just above. You should see the surface go shiny. Then you can adjust your flame back to encase or just it leave on the surface. Don't put the unencased bead back in a neutral flame or you'll undo it. For some of them you get different effects if you reduce them multiple times.

The Tartan Trout

Thank you. Will go try now and see what happens. :) :)

Lotti

I have just had exactly the same problem, even though I had read this post before!!!!!  ::) Think a little tuition on this one might be necessary for me, thankfully have got some sorted!  Hope you managed to do it Sarah, forgot to ask you yesterday. :)