chipperpottery

I really like doing ocean beads with lots of bits in them, but I can't seem to encase over a murrinii without it going out of shape.
Sometimes I don't mind, because I want them to look like little shells, but as my focals have a lot of glass I need to heat them so they do not crack but then I lose my nice round murrini?Advice please  ???

Les

I tend to heat the bits of my big beads in between the detail and hope that the heat will radiate throughout the bead.
Do you just decorate one side of your beads ? I blast the back side of my beads when there is just decoration on the front :)

Redhotsal

You could try "spot encasing" the murrine? After you've applied the murrine get a good hot gather of clear and press it down right over the top of the murrine. Don't swipe it across as that will smear it - but go straight down. Melt that in slowly - don't hold the murrine at an angle or the glass will droop and that may smear it again. Then encase as normally. Alternatively you can spot encase all of the bead instead of trying to coil encase.

By the way  - always wait until the base bead - including the murrine is cool enough to be rock solid if it will smear simply because it is too hot.

Billie

I've been scared to use the wonderful murrini I have from Kaz and Sabine for the same reason, but will give it another play now  :)  Thanks for the tips.

chipperpottery

I have pattern on all sides, thanks Sal I will try spot encasing them.