is the new bead rack in the bead cube causing my problem with aurea?

Started by sarah t, November 29, 2010, 04:21:41 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

sarah t

aurea has stopped doing its shine thing ??? .....not had a problem with it before ...

i read through previous posts and this one came up ..... (it suggested i started a new thead as was a bit old but if a mod wants to add it to the end of this thread feel free )

http://www.frit-happens.co.uk/forum/index.php?topic=21588.0

lee suggests a '' foreign object'' coud cause a change

the only thing changed is the new bead rack ....could this have caused the change in atmosphere in the kiln ?.....and will carbon /charcoal put it back to how it was ?



Lush!

I've successfully had shiny Triton since adding the bead rack to my Cube, but it wouldn't hurt to try the carbon thingy I suppose.


www.lushlampwork.etsy.com

turnedlight

Take the bead rack out and test your theory. :)
Personally I've never used a bead rack in my kiln, I might be missing out but I haven't noticed  ;D
kathryn