First beads - which colour glass?

Started by kibbutzangel, November 13, 2010, 10:39:24 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

kibbutzangel

I'm hoping to attempt my first bead tomorrow  ;D

I have a pack of assorted rods from Tuffnells, but have no idea which colour would be best to start out with, and whether I should use a 'solid' rod or a 'see through'.  Any advice appreciated, please!
Practice makes perfect ;)

Lush!

Blue is good.  It tends to be a 'what you see is what you get colour' and its easy to read the temperature change as the blue comes back very quickly as the glass cools.  I usually start my students with periwinkle blue for their first few beads.

I'd suggest avoiding white for your first few beads as its very soft and can be hard to control; also I'd avoid anything in the red family (inc oranges, yellow) as they look black until they're cool again.


www.lushlampwork.etsy.com

Redhotsal

They're just all a bit different. Opaque ones tend to be runnier - the runniest are white and ivory. See-through (transparents) are stiffer - the stiffest is probably cobalt blue and so you'll have to heat them up more to get the same degree of "runny-ness".
Some of them will "boil" easily - like yellow, so you'll have to work it higher in the flame.
I usually start students with something about half way between stiff and runny - like periwinkle blue or mid-turquoise - which are both opaques.
The important thing is to just play with the glass - don't over analysis what you're doing, and just have fun.
Exciting!  :D

Lush!

Quote from: Redhotsal on November 13, 2010, 10:53:18 PM

I usually start students with something about half way between stiff and runny - like periwinkle blue

Snap  ;D ;D ;D 

(probably another habit I picked up from you, Sal!)


www.lushlampwork.etsy.com

Redhotsal

we posted at the same time - so great minds think alike.  ::) ;)

kibbutzangel

Excellent!  Thanks ladies, just what I needed.  Just checked and I have a rod of that :D  Oooh, all excited!  I'll post a pic of the first just to give you all a reminiscence lol
Practice makes perfect ;)

Margram

Have fun and don't worry about odd shapes to start with - you'll soon improve as you practise ;D
Marg x  Etsy Flickr My blog

Blue Box Studio

Quote from: Margram on November 14, 2010, 01:13:03 PM
Have fun and don't worry about odd shapes to start with - you'll soon improve as you practise ;D

You need those odd shaped ones to go in the bottom of the bead release pot so they act as a mixer when you shake it.  Well, that's what I tell myself anyway!  I am evidence that you can fool some of the people all of the time.  ;D
Sue
Website ~ Etsy ~ Blog ~ Flickr

stuwaudby

To start I would suggest transparent Cobalt blue, transparant Greens, transparant Ambers or black. All these colours give a good indication of what temperature and viscosity they are at.

Beginners should avoid:
Clear - no indicaiton of melting.
White - colour changes to clear well above melting point, awkward to get a good shape.
Ivory - very quick to melt and can take ages to set again.
Reds - usually go grey and need to be striked (cooled and re-heated) to get the colour back.

princess pink

i used blues when i first learnt. periwinkle still remains a fav but i must use it more!

Fruddy

Quote from: Blue Box Studio on November 14, 2010, 05:10:08 PM
Quote from: Margram on November 14, 2010, 01:13:03 PM
Have fun and don't worry about odd shapes to start with - you'll soon improve as you practise ;D

You need those odd shaped ones to go in the bottom of the bead release pot so they act as a mixer when you shake it.  Well, that's what I tell myself anyway!  I am evidence that you can fool some of the people all of the time.  ;D

I do that as well!  Plus I always keep all my "Fuglies"..... they are a benchmark for your continued improvement.

noora

I used a lot of transparent green because green is one of my favourite colours :) I think it's good if you like the colours you use at the beginning, so that you'll like the results even if the shapes are a bit off. Just avoid the difficult colours mentioned above.