Making a set of beads in exactly the same size - Arrrrghh!

Started by Fruddy, November 06, 2010, 05:24:19 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Helen G

I made a sample bead the size I wanted on an undipped mandrel so it was permanently on there and annealed it. Then I used it as a visual guide for the set by holding each subsequent bead next to the the sample one and checking for size.

Kaz

The difficulty is of course that cold glass is smaller than hot glass!
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Trudi

Quote from: Kaz on November 06, 2010, 10:50:01 PM
The difficulty is of course that cold glass is smaller than hot glass!

Just what I was going to say!

Helen G

agreed, but the set in the kiln still turn out the same size as each other. Maybe should have pointed out they'll be slightly smaller than the sample bead  :-[

Sulis (Hazel)

It's a good idea Helen  ;D

Just echoing what the others said really...it's a combination of good ideas like reference beads and marking mandrels, plus PPP. Several years down the line I'll still struggle to make a set of exactly the same size beads if I shape by hand, - but then I don't make beads every day so I guess if I practice more I'll get there  ;D
Hazel x

AnnaSpanna

Quote from: Kaz on November 06, 2010, 10:50:01 PM
The difficulty is of course that cold glass is smaller than hot glass!

this is true but to be fair the difference in size for 104 glass is something like 0.0000104mm (or percent - can't remember which) per 1cm3 for every 1 degree C rise in temp so its not exactly massive... but PPP  ;D

Kaz

Are you sure Anna - because when I pull murrini there is a massive difference between the pull diameter when it's hot and when it has cooled thoroughly?
Or is it that glowing glass appears bigger?
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Pam


[/quote]
this is true but to be fair the difference in size for 104 glass is something like 0.0000104mm (or percent - can't remember which) per 1cm3 for every 1 degree C rise in temp so its not exactly massive... but PPP  ;D
[/quote]
But the eye just could not detect this level of difference and I too notice the difference when making several spacers on one mandrel.
But maybe as Kaz says the glow gives the appearances of a molten glass being bigger than cool glass?

Redhotsal

I have a pair of metal calipers and slip the hot bead through the gap to check. This makes things super accurate. I used to do it by eye, which was also pretty good - I can tell you how big 13mm or 16mm is just by looking now. I suppose that does come with practise.

I happen to think that unless a customer particularly demands it it's nice to have a little variation in size. We're making handmade things for goodness sakes - we may as well be machines if we spend all day using presses and shapers.

Okay - I'll concede that people who like their Pandora style beads want them all the same size but most other people are happy to have a nicely matched but size graduated set of beads.

AnnaSpanna

I just wrote a big reply to this and now its gone.... has anyone seen it?  Ok it went along the lines of:

hot glass is less viscous than cool glass thus has entirely different properties due to the very nature of glass as a material. The fact that glowing glass is simply so hot will also effect the air in the immediate vicinity of the bead and thus distort the image we have of it (all fuzzy, blobby and rounded generally). The teeny tiny figure I quoted needs to be multiplied by between 800-1100 as that is at what temp we heat our glass to to make it do its thing - this is still very tiny but significantly different to looking at the figure of COE as a simple formula against 1cm3 of glass at 1degree C.

Def way too technical for a sunday morning. I'm off to go melt some glass now!


Kalorlo

I tried putting a dot with permanent marker on some of my mandrels, below where the bead release would be, so that I could tell how many wraps I'd done without losing where the start point was. It didn't help a huge amount because my individual wraps aren't that similar in size!

If you're making simple beads you can try doing a pair to a mandrel, so you can compare them to each other. But yeah, mainly just practice - I can make a number that are fairly close in size now.

Also, if you've got a doming block, that can help if you compare them against the same dip, maybe roll them gently in it.

SilverGems89

i use my doming block, make a bead the size of a hole, then if it needs to be bigger i count the number of wraps i add, being as its only usually a few, but after the first few i can eyeball the size easily! It is just the old hat of PPP and then one day you'll just find it clicks!

turnedlight

funny enough, my core beads usually turn out the same size as each other, unless I fluff something and then do a salvage operation! I wouldn't be very receptive to a customer wanting a set where they are all identical, for me it would take the point (and the fun) out of handmaking my own beads. Having said that some of the beads I really admire and drool over are very precisely made :)
kathryn

Redhotsal

Oh, the other thing I do, if the beads are relatively simple, is to make them on the same mandrel. It's always a challenge to keep everything hot. Works great for simple spacers and earring pairs though.

JaySpangles

I sometimes make 2 spacers on one mandrel (when I'm feeling brave), and the second one always looks a bit bigger than the first until it has cooled a bit.
Apart from beadrollers I found an ancient pair of calipers in the garage and I find it a great help.