Supporting beads in wire mesh for a batch anneal

Started by ShinySnail, November 02, 2010, 10:01:14 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Steampunkglass

It does sound like galvanised to me too  :-\ Stainless steel is best really, I got a offcut strip which I bent in two in my kiln to rest mandrels on, been in there since I've bought the kiln (so a good two years) and it's still fine

ShinySnail

Ahhha have done a lot of investigating, unfortunately the B&Q mesh is deff not suitable (called the manufacturer)

Helen's site looks really good, will go for the stainless steel one on there...

Maybe i'll buy a chicken so my other mesh doesn't go to waste!
:D