Exploding beads

Started by Passionatelamper, October 08, 2010, 09:39:22 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Passionatelamper

Ok so I admit it, I have not had a good day today.....too long to go into.
So tonight I thought I would chill out and do beads even though I am totally exhausted.
Wrong decision!! has anyone experienced this please?
Beads kept exploding...nothing was going right, I thought I would use up some of the short ends I have left...My goodness me... I was being aimed at from all directions, can anyone explain this to me?
Nothing was going right...Could it be that the rods that were small and all in a box maybe were cracked or something?
Being a newbie I was a little worried what was going to happen next.
Maybe I should call it a day and go to bed with my Horlicks..
I am so mad at myself...I did manage to get a frog on a bead done, but even he looks sick!!
Not been at this lampwork for long I love it to bits, but maybe tonight I should have just sat down and read my 'Passing the flame' Will try again tomorrow...
I want to do all these beads and nothing was coming to me tonight.
I think the moral of the story is don't do lampworking when your knackered.
Nite all xxx

etsy-header-dec12 by vonnie.t, on Flickr

♥♥Tan♥♥

Are you saying the actual beads were exploding or the shorts you were using to make the beads? I have never heard of beads exploding except when they are left to cool for too long and are put back into the flame?

Passionatelamper

Yes there was a loud pop and then they fell apart I was working as normal..I don't really understand it to be honest..3 times in a row it happened I was puzzled.  :-\

etsy-header-dec12 by vonnie.t, on Flickr

Jolene

The beads that made a loud pop and fell apart? Maybe they were out of the flame for too long while you were selecting what shorts to use? The only time I have had a bead behave like that was, like Tan said, introducing it back in to the flame when it is too cool.

beadysam

Yep, the only time I've ener known it happen is when a bead is too cool.  The only other thing I can think of (a very long shot!) is the warm but damp weather effecting the bead release?... :-\

Kaz

Or your propane is on its way out and the beads not hot enough in the radiant heat and therefore cooling whilst on the mandrels?
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

lampworklover

Where is your torch? Might it be a draught?

When I first started I was in the dining room at my old house, and had to work with the patio doors wide open as ventilation. I had a hollow and a couple of discs pretty much do the same 'exploding' thing when the wind blew through if someone opened the other doors. ( I am now lucky enough to have a proper studio with proper ventilation, and it hasn't happened in there).


Passionatelamper

Ah I think that was it Tina as the window was open to my right behind me blowing the torch flame...it cannot be the propane as I have not had it long I think it was the draft from the window..... thank you

etsy-header-dec12 by vonnie.t, on Flickr

Passionatelamper

As an after thought what does everyone do with their short?

etsy-header-dec12 by vonnie.t, on Flickr

dangerousbead

I put them in a box and promise myself I will get a rod holder . . . one day.  :-)

Lyn G

If you melt it onto the end of another rod of the same colour when it gets down to about 3 or 4 inches, you will never end up with lots of shorts.   :) :)


Passionatelamper


etsy-header-dec12 by vonnie.t, on Flickr

Kalorlo

I've started making mine into stringer as I need it: I've got some of Maria Louisa's stainless steel chopsticks, so I melt the entirety of the short onto the end of one chopstick in a plug shape, then attach the other chopstick and pull it all out. Leave it for a minute and it'll just fall off the ends of the chopsticks as they cool. Then cut/break it into usable lengths. The ends that were on the chopsticks will have little cup shapes - you can just throw those away as they're utterly miniscule amounts of glass and probably have black stuff on the inside from where they were attached.  :)

SilverGems89

I save my shorts with the view of one day fusing them  :)