My Mandrel Broke?

Started by ShinySnail, July 23, 2010, 10:12:33 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

ShinySnail


Last night a bead I was making just fell to the desk, and when I looked I realised the mandrel had snapped.

Is this something that happens sometimes or have I done something that may have caused this?

???

hollergrafik

sounds like you have over heated the mandrel and melted it, I did this on a couple of occasions when I was starting out.

Dragonfire Glass

I think we have all melted througha manderel at some time!

ShinySnail


Ahhhh thanks, yeah it was quite a big bead, and I had spent a while on it...

Didn't realise that I could do that - oops!

Thanks for the info

flaming beads

Yup...i'm part of that club too :D....have kept it to remind me ;)