Do your beads crack if you batch anneal?

Yes always
0 (0%)
Only sometimes
4 (50%)
Never
3 (37.5%)
Other
1 (12.5%)

Total Members Voted: 8

princess pink

Well I'm considering buying a Bavarian heart press as a post exam treat but I batch anneal and need to know whether my beads will survive...

... So can anyone shed some light on this/advise how to stop the beads cracking?

Or would anyone be willing to lend me a Bavarian 3d m heart press any time from last week in august to mid sept?

helbels

I rarely get cracked beads and I batch anneal everything.  I use Manda's Annealing Bubbles which are fantastic, and can even get away with relatively large lentils.

Krysia@No98

Quote from: princess pink on July 22, 2010, 02:50:43 PM
Well I'm considering buying a Bavarian heart press as a post exam treat

You're fully focused on that revision I see  ;)
-* -  Courage is going from failure to failure with out loosing enthusiasm -*-

Trudi

I have a 3D one on way to me - I can try it out for you!

princess pink

Lol at krysia, yup but taking well deserved breaks!


Trudi that would be fab! I would love to see how you get on.

Helen, I've found that 28mm lentils crack with annealing bubbles which is a bit annoying, I've only had 1 that hasn't cracked on me yet, but maybe I let them get too cool!

helbels

I don't make really big lentils, I think 22mm is the biggest I've done.

Krysia@No98

Quote from: princess pink on July 22, 2010, 03:27:37 PM
Lol at krysia, yup but taking well deserved breaks!

;D It's only coz we love you  ;)  ( I have just noticed that Julie has commented too )
-* -  Courage is going from failure to failure with out loosing enthusiasm -*-

Nikki

I have the Bavarian puffy heart press have made about 20 hearts all cooled in Mandas annealing bubbles, not had any crack. This is the one I have.
http://www.bavarianbeads.com/product_info.php?cPath=24_59&products_id=335

Nikki


Nikki

I think it's worth a try, I would recommend the annealing bubbles if you don't already have them ;D

Trudi

Quote from: Trudi on July 22, 2010, 03:04:46 PM
I have a 3D one on way to me - I can try it out for you!

well I can report that it survived the blanket!!! It's now in the kiln!!!

Fab press, I love it!!!

princess pink

Quote from: Nikki on July 22, 2010, 08:57:21 PM
I think it's worth a try, I would recommend the annealing bubbles if you don't already have them ;D

i do have annealing bubbles but to be honest, i don't think they're that great for larger beads over 25mm. Bar one i've had every single bead over that size crack in annealing bubbles, but hardly any in the blanket. maybe i'm doing something wrong.

princess pink

Quote from: Trudi on July 24, 2010, 09:24:33 AM
Quote from: Trudi on July 22, 2010, 03:04:46 PM
I have a 3D one on way to me - I can try it out for you!

well I can report that it survived the blanket!!! It's now in the kiln!!!

Fab press, I love it!!!

oooo well that is exciting to know! I just managed to snap up the UCBY cindy heart press from rachel so may have to wait a bit for the bavarian one ( or borrow one ;) )

can't wait to see your beads trudi! ooo did you leave em on the mandrels?

Trudi

Hi yes, left on mandrels!!!

Perhaps after you've had a play with your heart press we could do a swap for a while!!!

princess pink

Quote from: Trudi on July 24, 2010, 12:40:22 PM
Hi yes, left on mandrels!!!

Perhaps after you've had a play with your heart press we could do a swap for a while!!!

Lol I think everyone is itching to get there hands on it! But yeah I'd be up for that.

I think my problem is I always take em off the mandrake. Maybe I should try and work out how to use te mandrel rack for my sc2!!