Losing the Reduction in a Maxi

Started by Lush!, June 19, 2010, 08:57:29 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Lee - Kilncare

Doh!!!!!!!!! So I was, O.K. I'll put it on the priority list.
Completely forgot about the photos mate. If just taken another look at them.

We'll get it sorted post haste!!

TWITTER @kilncare
VISIT US ON FACEBOOK FOR THE LATEST ON US.
http://www.facebook.com/pages/Stoke-On-Trent-United-Kingdom/Kilncare-Ltd/238801689732

Lee - Kilncare

#16
You should be careful about showing of yer m***** in public pal ;D

TWITTER @kilncare
VISIT US ON FACEBOOK FOR THE LATEST ON US.
http://www.facebook.com/pages/Stoke-On-Trent-United-Kingdom/Kilncare-Ltd/238801689732

Lush!

Quote from: Lee - Kilncare on June 21, 2010, 09:59:24 AM
You should be careful about showing of yer minge in public pal ;D

Ooh er!

Quote from: julieHB on June 21, 2010, 09:51:34 AM
but have you measured the actual temperature?

Nope!  I don't have the technology - but I think I'll have a go at lowering the temp and see what happens.



www.lushlampwork.etsy.com

Lee - Kilncare

Quote from: Lush! on June 21, 2010, 10:14:33 AM
Quote from: Lee - Kilncare on June 21, 2010, 09:59:24 AM
You should be careful about showing of yer m***** in public pal ;D

Ooh er!

erm....the door seal......good grief....some peoples minds ;D ;D

TWITTER @kilncare
VISIT US ON FACEBOOK FOR THE LATEST ON US.
http://www.facebook.com/pages/Stoke-On-Trent-United-Kingdom/Kilncare-Ltd/238801689732

Kaz

OH the fringe ;D
My curtains are looking a bit bare these days too Lee - can we buy replacements?
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Redhotsal

Kaz is posh - she has a fringe!  ;)

I'll show off my m**** with pride to all members of the public!  ;D ;D ;D ;D

Lush!

Update - I adjusted my temp down to 510 and made three little triton spacers, I put one on the left, one on the right and one in the middle of the kiln.

They've all come out with some shine (as opposed to none last time!) - the one on the right has fared best.

So once I've got my new er ... frilly bit ... I should be back to normal  :D


www.lushlampwork.etsy.com

Lee - Kilncare

Ahh great news mate. Keep us informed.

And Hi Kaz, click on the item you want off the MAXI page and you shall have  ;D
http://www.kilncare.co.uk/kilns_glass_beadannealing_maxiprofessionalkiln.html

TWITTER @kilncare
VISIT US ON FACEBOOK FOR THE LATEST ON US.
http://www.facebook.com/pages/Stoke-On-Trent-United-Kingdom/Kilncare-Ltd/238801689732

Redhotsal

I think we worked out before that the coolest part of the Maxi is on the right, the middle is the hottest and the left is "middle" - so to speak. Sarah Downton has more detailed information on this as she has "mapped" the temp along the Maxi - and although each kiln will vary a little, overall they all have the "hotspots" and "cool spots" in the same approximate areas. She can confirm/refute this - I can't actually remember exactly.
So, it would imply that you need to go down in temp a little bit more - as you got more shiny at the cooler end (that's me - technical to a "T") I actually operate my Maxi at "490" as I believe it is actually a bit hotter in the kiln than where the temperature is measured at the pyro.

silverlemon

Yep Sal, spot on. The right is low, the left is middle and the centre is top, lol  ;D

I garage at 465, I anneal at 483 and switch off at 320.

This gives a much higher temp at the centre.

I love the variation as I know I can keep stuff cooler at the right, eg Rubino, medium at the left, and if I want to kiln strike something more I shove it at the middle. Works every time  ;D
Bionic Sarah xxx    Sarah Downton On Facebook  My Etsy Shop

Lush!

Thanks Sal and Sarah.

I know you've mentioned this before but I can't ever get my head round stuff like this till I need to .. and now I need to and it all suddenly makes sense!


www.lushlampwork.etsy.com

Redhotsal

Yeah - I quite like having the variation too - makes the kiln much more versatile.