Hi there,  Ive got the kiln programed now,  I had set it to garage for 6 mins instead of 6 hours ::).  now I cant get it to skip to the annealing stage,  its an SC2.  I have pressed the up button to get SStP to show, and then press start,  but it says hold for a minute or so and then goes back to where it was before, ???  any ideas on what Im doing wrong please?
Thanks
Wendy in Essex

SallyR


You're almost there - just need to press Start again.

So from your garaging segment:

Press the Up arrow - SStP shows

Press Start - the number of the current garaging segment shows (HLd x, where x is whatever your garaging segment number is - mine says HLd 2)

Press Start again - this will skip the rest of the garaging segment and start the ramp to the annealing segment - you should see the temperature start to change so you'll know it's worked

Hope this helps
Sally
Experience is what you get when you don't get what you want ...

Pat from Canvey

When I ask DH to skip the kiln for me, (cat sitting comfortably on my lap) I keep it simple and say"press middle button once, left hand one twice)