Lettered Murrini - Cane

Started by Hels4444, March 14, 2010, 08:11:21 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Hels4444

Does anyone know a good tutorial or if anyone sells murrini in letters I need a J and a N??????? 

Mary

The Kimberley Adams book shows you how to build alphabet murrini, which order to build them, if that's any help.

Hels4444

Thanks Mary I will look it up, I have a feeling I am gonna find this hard!!!!!

helenfc

i think cindy jenkins book shows it too :)
good luck with it!

Redhotsal

They're not too difficult - but "O" is the easiest!

I could do 'em if you really want - but they're well worth having a crack at them yourself.

For J start with the inner section of the bit surrounding the J (i.e. make a closed U shape out of white). Then run black along the right hand side of the U from half way along the top to the bottom of the U. Encase with white up to the bit under the top of the J and then add a line of black to extend the top bit of the J out to the right. Encase in White all the way around and build this into a round shape by adding more white where necessary.

Hmmm.......that's difficult to put into words, so here's someone on Wetcnvas making some:

http://www.wetcanvas.com/forums/showthread.php?s=&threadid=84886

sarah t


Hels4444

Sarah and Sally thank you so much for your help  i have printed off both tuts and will spend some time over the weekend and see how I get on,  and Sally thank you so much for the back up offer I might be in touch if I cant master it!!!! ;D