Is my Tungston Rake really Tungston?

Started by SallyB, January 13, 2010, 11:00:12 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

SallyB

Hello

I wonder if someone might be able to help me.

I liked my stainless steel rake but the sticking annoyed me so I bought a Tungston one from Off Mandrel a while ago.  It sticks and I didn't think it would which makes me wonder if I'm doing something wrong or there's been a mistake (as seems to happen a lot to me with glass suppliers) and it's really stainless steel.

I'm mainly using it for pushing hot glass around to create beads like this:


Is there some way to tell if it's really Tungston?

Thank you for any help you may be able to give me.

Sally

Carl Martin

Stainless Steel will bend keep bending it and bending it and it will snap ~ metal fatigue.

Tungsten doesn't bend ~ if you try and it is tungsten, it will snap. It will take a bit of force but Tungsten has no memory and although super tough it is brittle.

Hope that helps.

Sam

Your pick might be sticking to the glass because it's hot.

Each time you use your pick on a hot bead you should cool it by plunging it in a small bowl
of water before touching the bead with it again.

As for knowing whether your pick is tungsten, can't help there I'm afraid ???

Hope this helps

Sam ;D

Redhotsal

If you put your tungsten pick really low in a very hot flame you will be able to get it to fume. Tungsten fumes are bright yellow. I dont' think I've seen steel act in the same way. Don't breathe in the fumes and make sure you have good extraction.
You can also try this- heat up the pick until glowing and then use the glowing pick to try and make a hole in the glass - if it's tungsten it will do this pretty easily. If it's steel you'll have great fun trying to extricate your pick from a molten glob of glass. Dunking the tool in water will clean off the hot glass.
You can rake your beads with any old steel tool - doesn't have to be tungsten. However, you need to avoid using the tool in direct flame - that's just a bad practice and will ruin your tools over time. Best way is to heat the bead up to glowing orange and then rake it, but out of the flame.

Ian Pearson

Sal is right about the yellow fumes off from Tungsten. Tungsten will stick to glass as will most metals I know. Under good working conditions boro can make an excellent seal and sometimes one can make a handle from glass bonded to tungsten rod to aid working although pin vices probably are better for some.

Ian

SallyB

Thank you very much for the advice
I'm not going to have a go at bending it.
I guess it probably is Tungston and I'm probably doing something wrong which is good because I can learn and fix my mistakes.
Thanks Sal, I'll try that fuming trick next time I'm out in the shed - hopefully it's tungston and I can correct my technique mistakes.

I really appreciate the help
thank you very much

Sally

Hamilton Taylor

If you have any doubts, please feel free to return it and we'll replace it free of charge.

Sean